[1] 曹志强. 硬脆材料液悬浮超光滑加工的理论与实验研究 . 长春:吉林大学 ,2007. CAO ZH Q. .Changchun:Jilin University,2007.(in Chinese)
[2] 王承遇,陶瑛. 玻璃的表面结构与性质 .http://www.cnki.net.
[3] WEYL W A. Structure of subsurface layers and their role in glass technology
[J].J. Non-Cryst. Solids,1975,19:1-25.
[4] WIEDERHORN S M,BOLZ L H. Stress corrosion and static fatigue of glass
[J].J. Am. Ceram. Soc.,1970,53(10):543-548.
[5] CHEN X P,XUAN B,WANG P,et al.. Study on the influence and disposal method of the micro-cracks of optical components
[J].SPIE,2009,7282:72820D/1-72820D/5.
[6] 王承遇,陶瑛 . 玻璃表面处理技术
[M].北京:化学工业出版社,2004. WANG CH Y,TAO Y.Processing Technology on the Glass Surface
[M]. Beijing:Chemical Industry Press,2004.(in Chinese)
[7] SAVIO G,MENEGHELLO R,CONCHERI G. A surface roughness predictive model in deterministic polishing of ground glass moulds
[J].Int. J. Mac. Tool.&Manu.,2009,49: 1-7
[8] TOMOZAWA M,TAKAMORI T. Relation of surface structure of glass to HF acid attack and stress state
[J].J. Am. Ceramic Soc.,1979,62(7-8):370-373.
[9] MELLOTT N P,BRANTLEY S L,HAMILTON J P,et al.. Evaluation of surface preparation methods for glass
[J].Surf. Interface Anal.,2001,31: 362-368.
[10] KISTLER S S. Stress in glass produced by nonuniform exchange of monovalent ions
[J].J. Am. Ceram. Soc.,1962,45(2):59-68.
[11] WONG L,SURATWALA T,FEIT M D,et al.. The effect of HF/NH4F etching on the morphology of surface fractures on fused silica
[J].J. Non-Crystal. Solids,2009,355:797-810.